Post B5EB8qOpt8zFwduei8 by fafo@social.fa-fo.de
 (DIR) More posts by fafo@social.fa-fo.de
 (DIR) Post #B5EB8qOpt8zFwduei8 by fafo@social.fa-fo.de
       1 likes, 3 repeats
       
       amogus-scale features now possible at fafo(behold, the sharpie lift-off process: scribble your substrate with a sharpie, deposit Al, dissolve sharpie with acetone)
       
 (DIR) Post #B5Fb9WD3ERopaALJ68 by skyguided@cathode.church
       0 likes, 0 repeats
       
       @fafo :blob_eyesdown: can you do indium tin oxide on glass?
       
 (DIR) Post #B5Fb9WcvgEWEsQRyQy by q3k@social.hackerspace.pl
       1 likes, 0 repeats
       
       @skyguided @fafo Should be doable. We'll see once we bring up our e-beam and sputter coaters... although thermal evap should still work to a certain degree.(and yes, making custom LCDs is somewhere in our tech tree :) )